Title: Anchorage Strength of Epoxy-Coated Hooked Bars

Author(s): Hamad, B. S.; Jirsa, J. O.; and D’Abreu, N. I.

Publication: Commentary Reference

Volume: 12

Issue: 13

Appears on pages(s): pp. 210-217

Keywords:

DOI:

Date: 6/1/2005

Abstract:
ACI Structural Journal, V. 90, No. 2, Mar.-Apr. 1993