Rectangular Concrete Stress Distribution in Ultimate Strength Design

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rectangular Concrete Stress Distribution in Ultimate Strength Design

Author(s): Mattock, A. H.; Kriz, L. B.; and Hognestad, E.

Publication: Commentary Reference

Volume: 10

Issue: 3

Appears on pages(s): pp. 875-928

Keywords:

DOI:

Date: 6/1/2005

Abstract:
ACI JOURNAL, Proceedings V. 57, No. 8, Feb. 1961