Maximum Crack Width in Reinforced Concrete Flexural Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Maximum Crack Width in Reinforced Concrete Flexural Members

Author(s): Gergely, P., and Lutz, L. A.

Publication: Commentary Reference

Volume: 10

Issue: 12

Appears on pages(s): pp. 87-117

Keywords:

DOI:

Date: 6/1/2005

Abstract: