238.1R-08: Report on Measurements of Workability and Rheology of Fresh Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 238.1R-08: Report on Measurements of Workability and Rheology of Fresh Concrete

Author(s): ACI Committee 238

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 70

Keywords: rheological measurements; rheology; workability; workability measurements.

DOI:

Date: 2/1/2008

Abstract:
This report provides a comprehensive view of workability of fresh concrete and a critical review of the tests available to measure workability and rheological performance of fresh concrete. The report discusses the factors affecting the performance of fresh concrete and provides a better understanding of the issues related to the design of workable concrete, from no flow (zero-slump) to flow like a liquid (self-consolidating concrete).