Title: Development of a High-Temperature Service Polymer Grout

Author(s): Akira Ohata and Giles Goldsbro

Publication: Symposium Paper

Volume: 128

Issue:

Appears on pages(s): 259-272

Keywords: compressive strength; epoxy resins; grout; workability; plastics, polymers, and resins; Materials Research

DOI: 10.14359/1917

Date: 11/1/1991

Abstract:
The paper briefly introduces experience with rotating machinery grouting, and the perceived need for a high-temperature service polymer-based grout material. It discusses design and handling parameters, and the development of a product that cures at ambient temperatures, without appreciable shrinkage, and has a compressive strength at 150 C of more than 40 MPa.