Contractors’ Guide to Mass Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Contractors’ Guide to Mass Concrete

Author(s): Bruce A. Suprenant and Ward R. Malisch

Publication: Concrete International

Volume: 30

Issue: 1

Appears on pages(s): 37-40

Keywords: bidding; cementitious materials; cracking; mass concrete; specification; temperature control.

DOI:

Date: 1/1/2008

Abstract:
To accurately bid a project, estimators need to know which structural components are considered mass concrete and the temperature limits that will apply. They also need to be familiar with the options available for keeping concrete temperatures within the limits so they can include the associated costs. A well-prepared bid includes a careful look at the specifications and an indication of the assumptions made when preparing the bid.