Five Discussions from the March/April 2007 ACI Structural Journal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Five Discussions from the March/April 2007 ACI Structural Journal

Author(s): Valter J. G. Lucio, Antonio P. Ramos, Himat Solanki, Narayan Swamy, and Dimitrios Theodorakopoulos

Publication: Structural Journal

Volume: 105

Issue: 1

Appears on pages(s): 111-116

Keywords:

DOI: 10.14359/19075

Date: 1/1/2008

Abstract:
Disc. 104-S13/From the Mar.-Apr. 2007 ACI Structural Journal, p. 123. Punching of Post-Tensioned Slabs - Tests and Codes. (Paper by Ricardo J. C. Silva, Paul E. Regan, and Guilherme S. S. A. Melo). Discussion by Antonio P. Ramos and Valter J. G. Lucio. Disc. 104-S15/From the Mar.-Apr. 2007 ACI Structural Journal, p. 142. Unified Shear Strength Model for Reinforced Concrete Beams - Part I: Development. (Paper by Kyoung-Kyu Choi, Hong-Gun Park, and James K. Wight). Discussion by Himat Solanki. Disc. 104-S16/From the Mar.-Apr. 2007 ACI Structural Journal, p. 153. Unified Shear Strength Model for Reinforced Concrete Beams - Part II: Verification and Simplified Method. (Paper by Kyoung-Kyu Choi and Hong-Gun Park). Discussion by Himat Solanki. Disc. 104-S18/From the Mar.-Apr. 2007 ACI Structural Journal, p. 170. Punching Shear Response of High-Performance Fiber-Reinforced Cementitious Composite Slabs. (Paper by Antoine Naaman, Visit Likhitruangsilp, and Gustavo Parra-Montesinos). Discussion by Dimitrios Theodorakopoulos and Narayan Swamy. Disc. 104-S19/From the Mar.-Apr. 2007 ACI Structural Journal, p. 180. Effect of Aggregate Size on Beam-Shear Strength of Thick Slabs. (Paper by Edward G. Sherwood, Evan C. Bentz, and Michael P. Collins). Discussion by Himat Solanki.


ALSO AVAILABLE IN:

Electronic Structural Journal