Title: A Whitetopped Driveway

Author(s): M. K. Hurd

Publication: Concrete International

Volume: 29

Issue: 12

Appears on pages(s): 38-39

Keywords: concrete overlay; paving; residential concrete; whitetopping

DOI:

Date: 12/1/2007

Abstract:
In 1990, the author had a cementitious whitetopping installed over the deteriorated asphalt driveway to her home. An update on the performance of the overlay after 17 years in service is provided in this article.