Air Pipe Cooling System

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Air Pipe Cooling System

Author(s): Shiro Ishikawa, Keisuke Matsukawa, Shigeki Nakanishi, and Hironobu Kawai

Publication: Concrete International

Volume: 29

Issue: 12

Appears on pages(s): 46-49

Keywords: cooling pipes; hydration; mass concrete; matt foundation; temperature; thermal control

DOI:

Date: 12/1/2007

Abstract:
A massive concrete foundation element in the hot and dry climate of Qatar required a concrete mixture that generated significant heat. To avoid excessive cracking, a construction procedure that incorporated air pipes in the foundation was used. Air pipe cooling was chosen over conventional water cooling because of the scarcity of water in the area, the large amount of energy required to cool the water, and the robustness and reliability of the system. Details of the analysis and construction are presented.