Toughened Throughout

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Toughened Throughout

Author(s): Philipp Hofmann, Darrell R. Mitchell, and Michael Chusid

Publication: Concrete International

Volume: 29

Issue: 12

Appears on pages(s): 40-44

Keywords: ballistic perforation resistance; blast resistance; high-performance concrete; micro-reinforced concrete

DOI:

Date: 12/1/2007

Abstract:
Micro-reinforced concrete incorporates multiple layers of three-dimensional fine steel mesh encased in a dense, high-strength mortar. Due to the material’s unique combination of properties, it’s already found acceptance in Europe for applications requiring resistance to blast, ballistic, impact, seismic, and other extreme loads. The unique properties of micro-reinforced concrete, which is now available in North America, and some of its current applications are discussed.