Experimental Verification of Strut and Tie Model Design Method

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Verification of Strut and Tie Model Design Method

Author(s): M. Tyler Ley, Kyle A. Riding, Widianto, Sungjin Bae, and John E. Breen

Publication: Structural Journal

Volume: 104

Issue: 6

Appears on pages(s): 749-755

Keywords: bearings; size effect; strut-and-tie modeling

DOI: 10.14359/18957

Date: 11/1/2007

Abstract:
Strut-and-tie models (STM) are a valuable tool for the design of irregular concrete members. This paper presents the experimental results of tests conducted on small-scale, simply supported dapped beams with openings under the load. The design of each test specimen was developed by independent student teams using the ACI 318-05 provisions for STM. An unreinforced specimen was also constructed for comparison. Each reinforced specimen resisted loads greater than the factored design load and exhibited little distress at service load levels. Examination of the behavior of each model permits appraisal of the design model used by each design team. These results show the STM to be a conservative, lower-bound design approach that allows the designer a great deal of flexibility.


ALSO AVAILABLE IN:

Electronic Structural Journal