Experimental and Analytical Progressive Collapse Evaluation of Actual Reinforced Concrete Structure

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental and Analytical Progressive Collapse Evaluation of Actual Reinforced Concrete Structure

Author(s): Mehrdad Sasani, Marlon Bazan, and Serkan Sagiroglu

Publication: Structural Journal

Volume: 104

Issue: 6

Appears on pages(s): 731-739

Keywords: brittle failure; dynamic structural analysis; integrity requirements; load redistribution; progressive collapse

DOI: 10.14359/18955

Date: 11/1/2007

Abstract:
One approach to evaluate progressive collapse of structures is to study the effects of instantaneous removal of a load-bearing element such as a column. In this paper, using experimental and analytical results, potential progressive collapse of an actual 10-story reinforced concrete (RC) structure following the explosion of an exterior column is evaluated. Development of Vierendeel action is identified as the dominant mechanism in redistribution of loads in this structure. The concrete modulus of rupture is identified as an important parameter in limiting the maximum recorded vertical deformation of the system to only 0.25 in. (6.4 mm). The changes in the directions of bending moments in the vicinity of the removed column and their effects such as potential reinforcing bar pullout (bond failure) are studied. Potential failure modes and their consequences are studied. Some shortcomings of integrity requirements in current codes are pointed out and effects of beam reinforcement detail on the development of catenary action are discussed.