Fourth International Workshop-Structural Concrete in the Americas

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fourth International Workshop-Structural Concrete in the Americas

Author(s): James R. Cagley and Shuaib H. Ahmad

Publication: Concrete International

Volume: 29

Issue: 10

Appears on pages(s): 35-38

Keywords:

DOI:

Date: 10/1/2007

Abstract:
The 4th International Workshop-Structural Concrete in the Americas took place April 20-21, 2007, in Atlanta, GA. Held in conjunction with the ACI Spring 2007 Convention, more than 80 experts from 21 countries participated. Special efforts were made to identify, select, and invite young practicing engineers as speakers. The technical sessions and recommendations from the Workshop are summarized in this article.