Title: SCM-24(07): Concrete Repair Basics

Author(s): ACI Committees

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 152

Keywords: anchorage; cementitious; coatings; concrete; joint sealant; placement; polymer; reinforcement; repair; cracking; strength evaluation; rehabilitation; survey.

DOI:

Date: 8/22/2007

Abstract:

Note: SCM-24(07) is No Longer Available.

This unique compilation of technical documents is used as technical reference material for ACI’s long-standing Concrete Repair Basics seminar and can be used as a general guide to concrete repairs. It includes copies of the following ACI documents: ACI 546R(04), Concrete Repair Guide; ACI 437R(03), Strength Evaluation of Existing Concrete Buildings; ACI 364.1R-07, Guide for Evaluation of Concrete Structures Before Rehabilitation; ACI 224.1R-07, Causes, Evaluation, and Repair of Cracks in Concrete Structures; ACI 201.1R-92(97) Guide for Making a Condition Survey of Concrete in Service. If purchased individually, the documents in this compilation are valued at over $245.


Product unavailable, please call +1.248.848.3800