Seven Discussions from the November/December 2006 ACI Structural Journal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seven Discussions from the November/December 2006 ACI Structural Journal

Author(s): Pradeep Bhargava, Mikael W. Braestrup, Shiming Chen, Sung-Chul Chun, Jinsheng Du, Taehun Ha, Sung-Gul Hong, Pinyin Lu, Bohwan Oh, Dipak Kumar Sahoo, Bhupinder Singh, and Himat Solanki

Publication: Structural Journal

Volume: 104

Issue: 5

Appears on pages(s): 638-646

Keywords:

DOI: 10.14359/18871

Date: 9/1/2007

Abstract:
Disc. 103-S79/From the Nov.-Dec. 2006 ACI Structural Journal, p. 783. Strain-Based Shear Strength Model for Slender Beams without Web Reinforcement. (Paper by Hong-Gun Park, Kyoung-Kyu Choi, and James K. Wight). Discussion by Himat Solanki. Disc. 103-S80/From the Nov.-Dec. 2006 ACI Structural Journal, p. 794. One-Way Shear Strength of Thick Slabs and Wide Beams. (Paper by Edward G. Sherwood, Adam S. Lubell, Evan C. Bentz, and Michael P. Collins). Discussion by Himat Solanki. Disc. 103-S81/From the Nov.-Dec. 2006 ACI Structural Journal, p. 803. On the Stress in Unbonded Tendons at Ultimate: Critical Assessment and Proposed Changes. (Paper by Mohamed H. Harajli). Discussion by Jinsheng Du and Pinyin Lu. Disc. 103-S82/From the Nov.-Dec. 2006 ACI Structural Journal, p. 813. Minimum Transverse Reinforcement for Bottle-Shaped Struts. (Paper by Michael D. Brown and Oguzhan Bayrak). Discussion by Dipak Kumar Sahoo, Bhupinder Singh, and Pradeep Bhargava. Disc. 103-S82/From the Nov.-Dec. 2006 ACI Structural Journal, p. 813. Minimum Transverse Reinforcement for Bottle-Shaped Struts. (Paper by Michael D. Brown and Oguzhan Bayrak). Discussion by Mikael W. Braestrup. Disc. 103-S82/From the Nov.-Dec. 2006 ACI Structural Journal, p. 813. Minimum Transverse Reinforcement for Bottle-Shaped Struts. (Paper by Michael D. Brown and Oguzhan Bayrak). Discussion by Sung-Chul Chun, Taehun Ha, Sung-Gul Hong, and Bohwan Oh. Disc. 103-S83/From the Nov.-Dec. 2006 ACI Structural Journal, p. 822. Behavior and Design of Adhesive Bonded Anchors. (Paper by Rolf Eligenhausen, Ronald A. Cook, and Jorg Appl). Discussion by Shiming Chen.


ALSO AVAILABLE IN:

Electronic Structural Journal