Title: Stress Analysis of Concrete Structures Subjected to Alkali-Aggregate Reactions

Author(s): Victor Saouma, Luigi Perotti, and Takashi Shimpo

Publication: Structural Journal

Volume: 104

Issue: 5

Appears on pages(s): 532-541

Keywords: alkali-aggregate reaction; dams; stress

DOI: 10.14359/18855

Date: 9/1/2007

Abstract:
In a separate paper, the authors have presented a constitutive model for the alkali-aggregate reaction (AAR) in concrete. This follow-up paper first examines how this complex and coupled model can be used for the long-term (until reaction exhaustion) prediction of an AARaffected concrete structure. Then, through a series of parametric studies, sensitivity analyses are performed, and then basic modeling questions are addressed. Finally, the effect of AAR on the structural behavior of two dams and a reinforced concrete structure is presented.