Title: Concrete Cover to Reinforcement — Or Cover Up?

Author(s): Adam Neville

Publication: Concrete International

Volume: 20

Issue: 11

Appears on pages(s): 25-29

Keywords: construction; cover; durability; reinforcing steels;

DOI:

Date: 11/1/1998

Abstract:
Discussion of the purpose of concrete cover over the steel reinforcement is presented. Three types of construction practice problems are identified with respect to durability: cover incorrectly specified, specification incorrectly formulated, and actual cover as specified. Article presents observed problems with cover in Canada, Australia, and Great Britain. Internationally recognized concrete expert suggests an improved approach so as to achieve the correct cover.