Precast Girders Prestressed with CFRP Wires - Hungarian Experiences

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Precast Girders Prestressed with CFRP Wires - Hungarian Experiences

Author(s): G.L. Balazs and A. Borosnyoi

Publication: Symposium Paper

Volume: 245

Issue:

Appears on pages(s): 73-94

Keywords: deflection control; FRP; pivot hysteresis; prestressing; serviceability

DOI: 10.14359/18763

Date: 4/1/2007

Abstract:
Use of non-metallic (FRP) reinforcements provides a promising alternative in order to avoid corrosion in reinforced concrete. By applying non-metallic (FRP) reinforcements there is no ferrous material to corrode in reinforced concrete. This paper reviews experiences with Carbon Fiber Reinforced Polymers (CFRP) for precast prestressed concrete girders. An experimental program was completed at the Budapest University of Technology and Economics, Faculty of Civil Engineering to study service behavior of precast concrete beams prestressed with CFRP tendons in terms of both load vs. deflection responses and cracking behavior. In this paper deflection control is presented with an introduction of a new simplified method and discussion of pivot hysteresis behavior under cyclic loading.