Title: Formwork Release Agents

Author(s): American Concrete Institute

Publication: Concrete International

Volume: 10

Issue: 6

Appears on pages(s): 43-45

Keywords: formwork (construction); oils; parting agents; waxes; Materials Research

DOI:

Date: 6/1/1988

Abstract:
Reviews the types of release agents and conditions affecting the choice of a release agent.