Statistical Acceptance Criteria for Strength of Mass Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Statistical Acceptance Criteria for Strength of Mass Concrete

Author(s): Ernest Schrader

Publication: Concrete International

Volume: 29

Issue: 6

Appears on pages(s): 57-61

Keywords: acceptance criteria; mass concrete; compressive strength; characteristic strength; dam

DOI:

Date: 6/1/2007

Abstract:
For structural concrete, the practice of requiring an average strength that will statistically assure that no more than a designated percentage of test results fall below a designated design strength has been adopted throughout the world. The concept is also applicable to dams, but it requires adaptation to the unique aspects of mass concrete. These aspects and examples of acceptance criteria for dam structures are presented following a discussion of the confusion between the internationally used term, characteristic strength, and U.S. terms used to describe concrete compressive strength.