SP-241: Concrete Heat Development: Monitoring, Prediction & Management

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: SP-241: Concrete Heat Development: Monitoring, Prediction & Management

Author(s): Editors: Kejin Wang and Anton K. Schindler

Publication: Symposium Paper

Volume: 241

Issue:

Appears on pages(s): 140

Keywords:

DOI: 10.14359/18614

Date: 4/1/2007

Abstract:
SP-241CD This CD-ROM contains nine papers presented at a technical session on Heat Development: Monitoring, Prediction, and Management, held in Atlanta, GA, in April 2007. Topics include innovative technology for concrete heat monitoring; use of the heat measurements to characterize concrete mixtures, evaluate the mixture performance, and detect potential incompatibilities of concrete materials; heat management in precast concrete; and modeling and prediction of in-place concrete temperature development, among others.