Repair Options for Curled/Warped Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Repair Options for Curled/Warped Slabs

Author(s): Scott Tarr and Calvin McCall

Publication: Concrete International

Volume: 29

Issue: 4

Appears on pages(s): 47-52

Keywords: curling; repair; slab-on-ground; warping

DOI:

Date: 4/1/2007

Abstract:
After providing a summary of the causes and functional effects of curling/warping of concrete slabs on ground, the positive and negative aspects of potential mitigation methods are discussed. These methods include cutting additional joints, grinding of edges, patching low zones, filling voids below the slabs, partial-depth concrete removal and replacement, and installation of dowels.