Title: Self-Curing Concrete, Why Not?

Author(s): Bryant Mather

Publication: Concrete International

Volume: 23

Issue: 1

Appears on pages(s): 46-47

Keywords:

DOI:

Date: 1/1/2001

Abstract:
In a letter in the September 2000 issue of Concrete International, D. Srinivasan asked, "Will there be a self-curing concrete?" My answer to this is strongly affirmative for three reasons.