Adsorption of Lignosulphonates on Cement and the Hydration Products of Cements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Adsorption of Lignosulphonates on Cement and the Hydration Products of Cements

Author(s): B.O. Myrvold

Publication: Symposium Paper

Volume: 239

Issue:

Appears on pages(s): 285-296

Keywords: adsorption; cement; clinker; hydration products; lignosulphonates

DOI: 10.14359/18385

Date: 10/1/2006

Abstract:
The adsorption of sodium lignosulphonate onto cement was investigated. The cement has either been pre-hydrated or hydrated with the lignosulphonate present. The pre-hydrated cement particles grow with time, thus a larger surface is created and the plateaus in the adsorption isotherms increase. With lignosulphonate present there is hardly any growth of new surface. It is found that, a lignosulphonate that adsorbs strongly to the surface causes, less retardation than weakly adsorbed lignosulphonates. This can be explained by different interactions with the different minerals present.