360R-06: Design of Slabs-on-Ground

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 360R-06: Design of Slabs-on-Ground

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 74

Keywords: concrete; curling; design; floors-on-ground; grade floors; industrial floors; joints; load types; post-tensioned concrete; reinforcement (steel, fibers); shrinkage; shrinkage-compensating; slabs; slabs-on-ground; soil mechanics; shrinkage; warping.

DOI:

Date: 8/9/2006

Abstract:

Note: A newer version of this document exists. This document was replaced by 360R-10.

This document presents information on the design of slabs-on-ground, primarily industrial floors. The report addresses the planning, design, and detailing of slabs. Background information on design theories is followed by discussion of the types of slabs, soil-support systems, loadings, and jointing. Design methods are given for unreinforced concrete, reinforced concrete, shrinkage- compensating concrete, post-tensioned concrete, fiber-reinforced concrete slabs-on-ground, and slabs-on-ground in refrigerated buildings, followed by information on shrinkage and curling problems. Advantages and disadvantages of each of these slab designs are provided, including the ability of some slab designs to minimize cracking and curling more than others. Even with the best slab designs and proper construction, however, it is unrealistic to expect crack-free and curl-free floors. Consequently, every owner should be advised by both the designer and contractor that it is normal to expect some amount of cracking and curling on every project, and that such occurrence does not necessarily reflect adversely on either the adequacy of the floor’s design or the quality of its construction. Design examples appear in an appendix.




  