Title: 117-06: Specifications for Tolerances for Concrete Construction and Materials and Commentary

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 70

Keywords: construction; concrete; drilled piers; formwork; foundation; masonry; mass concrete; pier; precast concrete; prestressed concrete; reinforced concrete; reinforcement; specification; splice; tolerances.

DOI:

Date: 8/15/2006

Abstract:

Note: A newer version of this document exists. This document was replaced by 117-10.

Specification synopsis: This specification provides standard tolerances for concrete construction. This document is intended to be used by specification writers and ACI committees writing standards as the reference document for establishing tolerances for concrete construction. Commentary synopsis: This report is a commentary on the Specifications for Tolerances for Concrete Construction and Materials (ACI 117). It is intended to be used with ACI 117 for clarity of interpretation and insight into the intent of the committee regarding the application of the tolerances set forth therein.