Experimental Study of RC Columns Strengthened with CFRP Sheets Under Eccentric Compression

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study of RC Columns Strengthened with CFRP Sheets Under Eccentric Compression

Author(s): W.-J. Yi, Q.-l. Xian, H.-T. Ding, and H.-y. Zhang

Publication: Symposium Paper

Volume: 238

Issue:

Appears on pages(s): 395-410

Keywords: CFRP; columns; eccentric loading; experiment; strengthening

DOI: 10.14359/18284

Date: 10/1/2006

Abstract:
The objective of this research project is to conduct an experimental study of the behavior of carbon fiber-reinforced polymer (CFRP) materials for strengthening reinforced concrete structures. The test program consisted of 23 reinforced concrete columns strengthened with CFRP sheets under static eccentric compressive loading. It is shown that under large eccentric compression loading, ultimate capacity of the columns can be effectively increased with the longitudinal CFRP sheets, and the ductility factors of the columns can be increased with the transverse CFRP sheets. It was observed that the material strength utilization of transverse CFRP sheets was more sufficient than that of longitudinal CFRP. The transverse CFRP sheets were broken at failure of a column, but the maximum measured strain in the longitudinal CFRP was only about 5000µe at peak load.