Experimental Study on Stress-Strain Relationship of Confined Concrete with GFRP Jackets

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study on Stress-Strain Relationship of Confined Concrete with GFRP Jackets

Author(s): C.D. Zhou and X.L. Lu

Publication: Symposium Paper

Volume: 238

Issue:

Appears on pages(s): 193-208

Keywords: analytical model; confined concrete; GFRP; stress-strain relationship

DOI: 10.14359/18272

Date: 10/1/2006

Abstract:
A two-stage analytical model for evaluating the stress-strain behavior of square concrete columns confined with glass fiber-reinforced polymer (GFRP) is proposed. Fifty-one square columns (divided into seventeen groups) were tested under static axial compression up to failure. The main factors considered in the test are as follows: grades of concrete, bonding shape, amounts of GFRP jackets, and space of fiber strips. The results clearly showed the efficiency of the GFRP jackets in enhancing the ultimate strain and the strength of the columns. The analytical model was calibrated using data from the tests, and good agreement between test and computation results was obtained.