Three Discussions from the July/August 2005 ACI Materials Journal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Three Discussions from the July/August 2005 ACI Materials Journal

Author(s): Ken W. Day, and William G. Hime

Publication: Materials Journal

Volume: 103

Issue: 3

Appears on pages(s): 218-220

Keywords:

DOI: 10.14359/18182

Date: 5/1/2006

Abstract:
Disc. 102-M24/From the July-Aug. 2005 ACI Materials Journal, p. 224. Sulfate Attack of Mortars Containing Recycled Fine Aggregates. (Paper by S. T. Lee, H. Y. Moon, R. N. Swamy, S. S. Kim, and J. P. Kim). Discussion by William G. Hime. Disc. 102-M25/From the July-Aug. 2005 ACI Materials Journal, p. 231. Three-Day Prediction of Concrete Compressive Strength Evolution. (Paper by Marco Viviani, Branko Glisic, and Ian F. C. Smith). Discussion by Ken W. Day. Disc. 102-M32/From the July-Aug. 2005 ACI Materials Journal, p. 279. Influence of Cation on Corrosion Behavior of Reinforcing Steel in High-pH Sulfate Solutions. (Paper by Laura Mammoliti and Carolyn M. Hansson). Discussion by William G. Hime.


ALSO AVAILABLE IN:

Electronic Materials Journal