Methods of Information Exchange in the Field of Prestressed Concrete Reactor Pressure Vessels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Methods of Information Exchange in the Field of Prestressed Concrete Reactor Pressure Vessels

Author(s): H. Benzler

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 1597-1620

Keywords: information centers; information retrieval; information systems; nuclear reactor containment; nuclear reactors; pressure vessels; prestressed concrete

DOI: 10.14359/18128

Date: 1/1/1972

Abstract:
A synopsis of the present methods of information exchange in the field of prestressed concrete reactor pressure vessels, particularly as handled by the Commission of the European Communities, is presented. Suggestions are also presented to aid the transfer of information.