Serpentine Concrete for Czehoslovakin A-2 Reactor Shielding

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Serpentine Concrete for Czehoslovakin A-2 Reactor Shielding

Author(s): A. Honig, F. Vessly, M. Samalikova, B. Stoces, and M. Havranek

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 1225-1242

Keywords: compressive strength; concretes; heavyweight aggregates; heavyweight concretes; high temperature; mechanical properties; moisture content; neutron sources; nuclear reactor containment; nuclear reactors; physical properties; radiation shielding; research

DOI: 10.14359/18112

Date: 1/1/1972

Abstract:
In this paper are presented results of geological prospecting and of testing physical and mechanical properties of serpentinite and ordinary concretes.