Title: Iron-Serpentine Concrete

Author(s): H.S. Davis

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 1195-1224

Keywords: gamma rays; grout; heavyweight aggregates; heavyweight concretes; high temperature; iron; metal scrap; moisture content; mortars (material); neutron sources; nuclear reactor containment; nuclear reactors; physical properties; preplaced-aggregate concrete

DOI: 10.14359/18111

Date: 1/1/1972

Abstract:
Data are presented on the phyical and nuclear shielding properties of two types of iron-serpentine concrete. Specimens were tested under standard conditions and after being heated at elevated temperatures up to about 320 C.