Some Peculiarities and Results of Investigations of Thermal Conductivity and Diffusivity of Heavy Concretes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Some Peculiarities and Results of Investigations of Thermal Conductivity and Diffusivity of Heavy Concretes

Author(s): A.E. Desov and L.F. Jankelev

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 1059-1068

Keywords: aggregates; granite; heavy-weight aggregates; heavy-weight concretes; limonite; magnetite; moisture content; nuclear reactor containment; radiation shielding; research; serpentine; temperature; thermal conductivity; thermal diffusivity

DOI: 10.14359/18106

Date: 1/1/1972

Abstract:
There are some attempts in this paper to overcome the difficulties in studying thermotechnical properties of heavy concretes. To exclude the influence of thermal contact resistance it is recommended to test the specimens of different thickness, placing the sample in intimate contact with the thermocouple and at last to use lubrication of the surface. Knowing the thermal conductivity of the lubrication and air one can calculate the real conductivity of a specimen under investigation.