Title: Thermal Conductivity and Thermal Expansion Coefficients of Concrete as a Function of Temperature and Humidty

Author(s): J.C. Marechal

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 1047-1058

Keywords: aggregates; concretes; desorption; diffusion; high temperature; humidity; low temperature; moisture content; nuclear reactor containment; research; temperature; thermal conductivity; thermal expansion

DOI: 10.14359/18105

Date: 1/1/1972

Abstract:
Thermal conductivity and thermal expansion coefficients were measured on various concretes according to temperature and the loss of water up to 500 C. The results are set out and discussed in relation to the other properties previously mentioned.