Title: Shrinkage, Moisture, and Pore Pressures in Heated Concrete

Author(s): G.L. England and A.D. Ross

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 883-908

Keywords: concretes; high temperatures; moisture content; nuclear reactor containment; nuclear reactors; permeability; pore pressure; pressure vessels; research; shrinkage; strains; thermal gradient

DOI: 10.14359/18098

Date: 1/1/1972

Abstract:
The paper describes some effects related to moisture in concrete, at elevated and nonuniform temperatures.