An Investigation of the Time-Dependent Behavior of Prestressed Concrete Pressure Vessels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: An Investigation of the Time-Dependent Behavior of Prestressed Concrete Pressure Vessels

Author(s): G.D. Whitman, J.P. Callahan, and J.M. Corum

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 823-846

Keywords: creep properties; high temperature; loads (forces); measuring instruments; models; moisture content; nuclear reactor containment; nuclear reactors; pressure vessels; prestressed concrete; research; strains; stresses; strucutral analysis; thermal gradient

DOI: 10.14359/18095

Date: 1/1/1972

Abstract:
The efffects of the thermal conditions imposed on a prestressed concrete pressure vessel (PCRV) present a major uncertainty in predicting long-term vessel behavior. In current vessel deesigns insulating and cooling are provided to limit concrete temperatures to 200 F (93 C) or less; however, the time-dependent behavior of the structures may be significantly affected by this relatively low temperature.