An Experimental Study of Multiaxial Creep in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: An Experimental Study of Multiaxial Creep in Concrete

Author(s): J.E. McDonald

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 735-768

Keywords: aggregates; axial loads; biaxial loads; chert; compressive strength; concretes; creep properties; deformatiopn; graywacke; high temperature; hydrostatic pressure; limestone; moisture content; nuclear reactor containment; pressure vessels; research

DOI: 10.14359/18092

Date: 1/1/1972

Abstract:
The purpose of this continuing investigation is to develop information regarding the time-dependent deformation behavior of concrete in the presence of varying temperature, moisture, and loading conditions similar to those encountered in a prestressed concrete reactor vessel (PCRV). This particular investigation is concerned with one concrete strength, three aggregate types, one cement, two moisture conditions, two testing temperature, and four loading conditions.