Title: Influence of High Temperatures on Strength and Deformation of Concrete

Author(s): H. Weigler and R. Fischer

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 481-494

Keywords: aggreagates; barite; compressive strength; concretes; deformation; heavyweight concrete; high temperature; moisture content; nuclear reactor containment; portland cements; quartz; research; slag cements; stress-strain relationships; thermal conductivity

DOI: 10.14359/18082

Date: 1/1/1972

Abstract:
This paper deals with the influence of high temperatures on the compressive strength and the deformations of concrete.