Title: Studies on the Technology of Concretes Under Thermal Conditions

Author(s): E. Crisping

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 443-480

Keywords: aggregate gradation; barite; compressive strength; concretes; creep properties; high temperature; limestone; modulus of elasticity; mortars (material); nuclear reactor containment; Poisson ratio; research; tensile strength; thermal conductivity

DOI: 10.14359/18081

Date: 1/1/1972

Abstract:
A research program sponsered by EURATOM to develop a concrete made of readily available components capable of being used at high temperatures as structural material for nuclear reactor pressure vessels is presented.