Title: Strength and Inelastic Propertes of Concrete at Elevated Temperature

Author(s): Noriaki Nishizawa and Hajime Okamura

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 407-422

Keywords: age; compressive strength; concretes; creep properties; high temperature; modulus of elasticity; nuclear reactor containment; Poisson ratio; prestressed concrete; research; strains; thermal expansion

DOI: 10.14359/18078

Date: 1/1/1972

Abstract:
Experiments on strength, Young's modulus, Poisson's ratio and creep of concrete exposed to elevated temperatures were carried out. Based on the results of experiments, strengths of sealed specimens stored at elevated temperatures and the creep strains of prestressed specimens exposed to elevated temperatures or exposed to cycles of temperature changes are described, and some problems in application of concrete for nuclear reactor are discussed.