Strength of Concrete Under Uniaxial Sustained Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength of Concrete Under Uniaxial Sustained Loading

Author(s): Siegfried Stockl

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 313-326

Keywords: age; compressive strength; concretes; creep properties; deformation; failure mchanisms; loads (forces); long-time study; Poisson ratio; research; strength; strains; stresses

DOI: 10.14359/18072

Date: 1/1/1972

Abstract:
Based on the results of 15 years of study, the strength of concrete under sustained loading is investigated. The strength of concrete subjected to long-time loads of varying magnitude and time is compared with the strength obtained with short-time tests.