Title: Concrete Strength in Multiaxial Stress States

Author(s): V. Hanson and K. Schimmelpfennig

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 295-312

Keywords: compressive strength; compressive stress; concretes; failure mechanisms; pressure vessels; prestressed concrete; research; strength stresses; tensile stress; triaxial loads

DOI: 10.14359/18071

Date: 1/1/1972

Abstract:
Presents a strength criterion for concrete in multiaxial compression. The strength criterion is based on biaxial and triaxial compressive strength tests on cubes, cylinders, and slabs.