Evaluation of the Influence of Some Concrete Characteristics on Non-Linear Behavior of a Prestressed Concrete Reactor Vessel

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluation of the Influence of Some Concrete Characteristics on Non-Linear Behavior of a Prestressed Concrete Reactor Vessel

Author(s): M. Hussain Khan and B. Saugy

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 159-180

Keywords: breeder reactors; cracking (fracturing); finite element method; loads (forces); nuclear power plants; nuclear reactor containment; nuclear reactors; pressure vessels; prestressed concrete; safety factor; shear properties; shells (structural forms)

DOI: 10.14359/18064

Date: 1/1/1972

Abstract:
Non-linear behavior up to rupture of wall of a PCRV, having large cylindrical vertical cavities for direct cycle turbines, have been examined with the aid of Finite Element Method.