Title: PCRV, Problems of Calculation, Material Properties and Evaluation of Results

Author(s): Hans H. Hofmann

Publication: Symposium Paper

Volume: 34

Issue:

Appears on pages(s): 141-158

Keywords: computer programs; cracking (fracturing); creep properties; deformation; high temperature; loads (forces); nuclear reactor containment; nuclear reactors; plastic analysis; pressure vessels; prestressed concrete; shrinkage; stress analysis; sresses

DOI: 10.14359/18063

Date: 1/1/1972

Abstract:
This paper is concerned primarily with stress analysis. Computer technilogy has presented the opportunity for approximation techniques and iterative procedures replacing the traditional systems of differential equations. The paper presents possibilites of structural analysis (material properties) which are necessary for assessment of structural behavior.