Shotcrete Payment Provisions, A Contractor's View

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shotcrete Payment Provisions, A Contractor's View

Author(s): J.S. Bhore

Publication: Symposium Paper

Volume: 54

Issue:

Appears on pages(s): 269-272

Keywords:

DOI: 10.14359/18033

Date: 1/1/1977

Abstract:
All of us here are, I presume, proponents of shotcrete in one form or another. I happen to be an advocate of sprayed concrete under all but the most unfavorable circumstances. However, being a supporter of shotcrete is not the issue here...payment for its application is.