Fatigue Strength of Reinforcing Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fatigue Strength of Reinforcing Bars

Author(s): Nils-Ove Gronqvist

Publication: Symposium Paper

Volume: 26

Issue:

Appears on pages(s): 1011-1059

Keywords: cyclic loads; deformations (reinforcing steels); fatigue (materials); reinforcing steels; research

DOI: 10.14359/18007

Date: 1/1/1971

Abstract:
In the present investigation, the steel quality and the profile of the reinforcing bars have been studied. . .Four different steel qualities, three types of bar profiles and two different degrees of wear on the part of the rolls have been studied.