Analysis and Design of Prestressed Concrete Circular Bow Girders for Bridge Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analysis and Design of Prestressed Concrete Circular Bow Girders for Bridge Structures

Author(s): Eduardo A.B. Salse

Publication: Symposium Paper

Volume: 26

Issue:

Appears on pages(s): 714-740

Keywords: bending moments; bow girders; bridges (structures); curved beams; girders; post-tensioning; prestressed concrete; prestressing; prestressing steels; structural analysis; structural design; torsion

DOI: 10.14359/17998

Date: 1/1/1971

Abstract:
The problem of prestressing a horizontally curved beam is studied in general. Horizontal and vertical eccentricities are considered in order to control simultaneously, torsional and bending stresses throughout the girder. . .It is pointed out that in such a case not only vertical but also horizontal cable eccentricities are required.