Experimental and Analitical Investigation of a Horizontally Curved Box-Beam Highway Bridge Model

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental and Analitical Investigation of a Horizontally Curved Box-Beam Highway Bridge Model

Author(s): I. Aneja and F. Rol

Publication: Symposium Paper

Volume: 26

Issue:

Appears on pages(s): 379-410

Keywords: box beams; bridges (structures); curved beams; finite element method; flexural tests; grider bridges; girders; models; prestressed concrete; reinforced concrete; research; strains; stresses; structural analysis

DOI: 10.14359/17985

Date: 1/1/1971

Abstract:
Currently, a large number of concrete highway bridges having box-sections with cantilevered deck slabs are being constructed. This paper presents an investigation of horizontally curved box-beam bridges through model analysis and experimentation. A plastic model was constructed and tested under various loading conditions.