Shotcrete Safety and Evironmental Control

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shotcrete Safety and Evironmental Control

Author(s): Robert C. Bates

Publication: Symposium Paper

Volume: 45

Issue:

Appears on pages(s): 130-142

Keywords:

DOI: 10.14359/17942

Date: 1/1/1974

Abstract:
Health and safety considerations in the use of shotcrete are discussed. The dust conditions, rebound problems, and causticity problems that occur during the shotcreting are discussed along with methods of overcoming them. There are also problems concurrent with shotcrete after it has been in place for a few minutes or several days. These include lack of strength, residual causticity, and improper placement.