Summary of Session III - European Shotcreting Practices

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Summary of Session III - European Shotcreting Practices

Author(s): Tor L. Brekke

Publication: Symposium Paper

Volume: 45

Issue:

Appears on pages(s): 96-100

Keywords:

DOI: 10.14359/17938

Date: 1/1/1974

Abstract:
This session met in the evening of Monday, July 16. There were only two invited speakers, both with experience from Scandinavia. This should be kept in mind when studying the comments below as they may not necessarily reflect the practices that prevail in other parts of Europe.